Figure 11. The relationship between Piezo1 and integrin β1. (A) Immunofluorescence detection of Piezo1 and integrin β1 on different matrix stiffness. (B) Statistical analysis of immunofluorescence intensity. *P<0.05,**P<0.01,***P<0.001. The expressions of both Piezo1 and integrin beta 1 increased with increasing stiffness, and were both highly expressed on 62-68kpa and low on 13-16kpa. n=3.